TROXYMITE
Is Durable
TROXYMITE's unique formulation is designed to actually strengthen the surface to which it is applied. Tests have shown that TROXYMITE is FIVE TIMES STRONGER THAN CONCRETE. The product is highly resistant to solvents, alkalis, salts and acids, making it the ideal protective topping where spillage of such industrial products occur.
TROXYMITE
Is Abrasion Resistant
"IT'S DIFFICULT TO GRIND AWAY!" An example of TROXYMITE's strong resistance to abrasion is in the grain storage industry. Grain Elevator Companies have saved hundreds of thousands of dollars in replacement costs by applying TROXYMITE in critical high-abrasive areas of their operations such as the interior of elbows of metal grain chutes. TROXYMITE is recommended for any rigid surface which must withstand high abrasive contact.
TROXYMITE
Adheres To Multiple Surfaces
The epoxy resin in TROXYMITE is one of the most adhesive substances known. TROXYMITE gives excellent adhesion on surfaces of wood, masonry, concrete, ferrous metals, most non-ferrous metals, and painted surfaces when the paint is securely bonded to the surface.
TROXYMITE
Is Quick Curing
A TROXYMITE surface is ready for traffic within 24 hours of application! A maintenance crew can lay down a new floor of TROXYMITE over the weekend and it will be ready for "business as usual" on Monday morning.
TROXYMITE
Is Economical
TROXYMITE is priced competitively with most other resurfacing and patching compounds, but due to its unique characteristics, TROXYMITE is in a class by itself. You get more for your money in strength, non-shrinking, safety, wear and chemical resistance with TROXYMITE.
TROXYMITE
Is Ready To Apply
By following the three basic steps - - - preparing the surface, mixing procedures and method of application found in the instruction sheet - - - TROXYMITE can be applied successfully with unskilled help.
Physical Properties Of TROXYMITE Compared To Concrete
TEST ? COMPRESSIVE STRENGTH: TROXYMITE - 13,500 lbs. per sq. in. (7 days) Concrete - 3,730 lbs. per sq. in.
TEST ? TENSILE: TROXYMITE - 2,900 lbs. per sq. in. (7 days) Concrete - 370 lbs. per sq. in.
TEST ? IMPACT STRENGTH: TROXYMITE - 14 ft. lbs. for ?" layers on concrete Concrete - 10 ft. lbs. for 2" layer
Two Textures
FINE: Product Code #3111
Cures to a smooth finish, the color of concrete. Slightly stiffer than Coarse Grain. Especially good for patching.
COARSE: Product Code #3110
Cures to a grainy finish and a light gray color. Easy to work with when surfacing large areas.
Rate Of Coverage
The coverage of TROXYMITE depends on the thickness of application and the condition of the floor. Under normal circumstances one gallon of TROXYMITE covers:
5 square feet at ?" thickness
10 square feet at 1/8" thickness
A pitted floor will require more TROXYMITE. Regardless of the size of the indentations, it takes additional TROXYMITE to fill these spaces
|